Which process would work best in outdoor condition that are very windy.
GTAW
GMAW
FCAW-G
SMAW
Which process would typically have the highest deposition efficiency without accounting for spatter loss.
SMAW
GMAW
GTAW
FCAW
A weld discontinuity that consists of weld metal that does not extend through the entire thickness single vee groove weld joint that is welded from one side only is called?
Porosity
Incomplete Fusion
Incomplete Penetration
Root convexity
Which of the following mild steel SMAW electrodes is considered low hydrogen
6010
6011
7010
E 7015 B2L
7024
The 7 in E71-T1 represents the tensile strength of the deposited weld metal
in PSI divided by 1000
in PSI divided by 10000
in PSI X 7
in PSI divided by 3.14159
A 1/8" 7018 has a core wire diameter of
3/32"
1/16"
.125"
.187"
Which of the following is the best approximate setting for a 1/8" E7018 welding a horizontal fillet weld on 1/4" material.
85
65
125
105
Which material has the highest thermal conductvity
Steel
Aluminum
Stainless Steel
Cast Iron
When welding with SMAW what type of power source is required
Constant voltage
Constant Current
Neither of the Above
Either of the Above
The Gas metal arc welding process using the short circuiting transfer mode using 18 volts using .035" ER70S-6 is best suited for
a 1/8" fillet weld on 3/16" thick lap joint.
a single vee groove weld in the flat position on 1/2" thick steel.